Keith,
Try using a fine grit of sand, something like #120 or #180, and slightly
increasing the ration amount of clay.
John
At 06:13 PM 4/25/99 -0700, Keith Breuker wrote:
>What is the method for troweling the final coat to get a tight,
>non-porous surface? I seem to be able to do this part of the time but
>not with any consistancy even within the same well mixed batch of
>material. Have tried various ratios of clay and sand. The bulk of the
>surface is porous and needs something like floor wax or polyurethane to
>seal the porosity.
>
>After sealing with two coats of Natural Choice linseed oil sealer a test
>coat of AFM polyurethane on a small area produced a nice smooth finish.
>
>
>--
>Keith Breuker - Engineer
>
>Straw Bale Owner/Builder
>Flyfishing Author
>Beulah, Michigan USA
>616 882-5648 flyfisherkb at centuryinter.net
>
John Swearingen
Skillful Means.....Architecture and Construction
we invite you to visit our web site at..........
http://www.skillful-means.com